20D Light gray polyester leather coreinner conductive

Textile Conductive Master Yarn At present, there are mainly the following three methods for the preparation of conductive polyester: one is to mix conductive particles into the spinning melt, and to make conductive polyester with skin-core structure or sea-island structure through composite spinning. The durability is very good, but the composite spinning process is complicated and the cost is high; the second is to use physical or chemical methods on the surface of the polyester to form a metal coating on the surface of the fiber. This method can produce conductive fibers with a specific resistance below 1028·cn . However, the formed metal coating often makes the fiber feel rough and hard, making it difficult for textile processing, and the production equipment investment is large, the efficiency is low, and the production cost is high; the third is to use chemical methods to form a semiconductor thin layer on the surface of polyester.Conductive Fabric Electrically conductive…